文献摘要

被引文献

相似文献

构建了由14规浇口蜡和各种规尼龙线组成的试验模型,并用于区分几种合金的浇注性。比较了7种商用低含金量陶瓷熔接金属修复体合金的浇注性能。五种用于全铸造修复体的商用低含金量黄色合金相互比较,并与III型认证对照进行比较。
A test pattern composed of 14 gauge sprue wax and various gauges of nylon lines was constructed, and used to differentiate the castability of several alloys. The castability of seven commercial low gold content alloys for porcelain fused to metal restorations was compared. Five commercial low gold content yellow alloys for full cast restorations were compared to each other and to a Type III certified control.