Soft X-ray Magnetic Circular Dichroism of a CoFe/MnIr Exchange Bias Film under Pulsed High Magnetic Field

Soft X-ray Magnetic Circular Dichroism of a CoFe/MnIr Exchange Bias Film under Pulsed High Magnetic Field
复制标题

脉冲强磁场下 CoFe/MnIr 交换偏置薄膜的软 X 射线磁圆二色性

DOI:
10.1143/apex.4.066602
复制
发表时间:
2011
影响因子:
2.3
通讯作者:
Hiroyuki Nojiri
Hiroyuki Nojiri
中科院分区:
物理与天体物理3区
文献类型:
--
作者:
Tetsuya Nakamura;Yasuo Narumi;Toko Hirono;Misaki Hayashi;Kenji Kodama;Masakiyo Tsunoda;Shinji Isogami;Hirokazu Takahashi;Toyohiko Kinoshita;Koichi Kindo;Hiroyuki Nojiri

文献摘要

相似文献

用非破坏性脉冲磁铁测量了在高达21 T的脉冲强磁场下的软X射线磁圆二色性。作为强磁场XMCD测量的一个例子,研究了Co 70 Fe 30/Mn 75 Ir 25双层膜中Co和MnL 2,3边的XMCD效应.采用总电子产额法检测吸收。吸收通过与50 ms高磁场脉冲同步的1 MHz时间分辨检测来记录。使用这种方法,XMCD效应由μ m(H)表示,这是磁场的函数。
Soft X-ray magnetic circular dichroism (XMCD) under pulsed high magnetic fields of up to 21 T has been measured using a nondestructive pulse magnet. XMCD effects at the Co and the Mn L 2, 3-edges of a Co 70 Fe 30/Mn 75 Ir 25 bilayer film have been investigated as an example of a high-magnetic-field XMCD measurement. A total electron yield method is adopted to detect absorption. Absorption is recorded by a 1-MHz time-resolved detection synchronized with a 50-ms high-magnetic-field pulse. Using this method, the XMCD effect is represented by µ m (H), a function of magnetic field.