A Novel MCFC Cathode Material Modified by the EPD Technique

A Novel MCFC Cathode Material Modified by the EPD Technique
复制标题

DOI:
10.1002/fuce.200330122
复制
发表时间:
2003-12
期刊:
影响因子:
2.8
通讯作者:
L.J. Chen;J. Zuo;C. Lin
L.J. Chen;J. Zuo;C. Lin
中科院分区:
工程技术4区
文献类型:
--
作者:
L.J. Chen;J. Zuo;C. Lin

文献摘要

被引文献

相似文献

阴极材料的早期变形已被证实是缩短电池寿命的重要因素。因此,非常需要一种既具有较低溶解度又具有较轻变形的新型阴极。在这项工作中,一种新型的复合材料,LiCoO 2-Ni,通过电泳沉积(EPD)技术制备,这是显着的,能够同时减少阴极材料的变形和溶解。事实证明,这对MCFC行业来说是非常有前途的。
The early deformation of the cathode material has been confirmed to be a significant factor in shortening the cell life. Thus, a new kind of cathode with both lower solubility and lighter deformation is highly desirable. In this work, a novel composite material, LiCoO2‐Ni, was prepared by the electrophoretic deposition (EPD) technique, which, remarkably, is able to reduce the deformation and dissolution of cathode materials simultaneously. It was demonstrated to be very promising for the MCFC industry.