Addition of fluoride compounds to acrylic resin plates: bending strength and fluoride release.

Addition of fluoride compounds to acrylic resin plates: bending strength and fluoride release.
复制标题

在丙烯酸​​树脂板中添加氟化物:弯曲强度和氟化物释放。

DOI:
10.1111/j.1365-2842.1981.tb00473.x
复制
发表时间:
1981
影响因子:
2.9
通讯作者:
R. Grajower
R. Grajower
中科院分区:
医学2区
文献类型:
--
作者:
A. Zitz;I. Gedalia;R. Grajower

文献摘要

被引文献

相似文献

研究了在丙烯酸树脂板中掺入CaF2(2.04%)、NaF(2.27%)和氟化胺(0.71%)对合成唾液中冲洗和浸泡的弯曲强度和氟化物释放量的影响。抗弯强度分别降低6.7%、9.5%和20%。氟化物从含NaF的板中释放最多,从含CaF2的板中释放时间最长,可能与化合物的溶解度有关。结果表明,AmF化合物的有机分子对亚克力板的强度影响最为显著。在体外冲洗实验中释放的F-浓度可以假定在体内由于牙科器具的较大尺寸而以较高的水平发生。
The effect of incorporated CaF2 (2.04%), NaF (2.27%) and amine fluoride (0.71%) in acrylic resin plates, on bending strength and fluoride release by rinsing and immersion in synthetic saliva, was determined. Bending strength was reduced by 6.7, 9.5 and 20% respectively. The most elevated release of fluoride from the NaF containing--and the most protracted from the CaF2 containing--plates may be related to the solubilities of the compounds. It appears that the organic molecule of the AmF compound affects the strength of the acrylic plates most significantly. The F- concentrations released in the in vitro rinsing experiment may be presumed to occur in vivo at some higher level due to the larger size of dental appliances.