Sub-180 nm generation with borate crystal
Sub-180 nm generation with borate crystal
复制标题
使用硼酸盐晶体的亚 180 nm 一代
DOI:
10.1016/j.optmat.2014.01.021
复制
发表时间:
2014
影响因子:
3.9
通讯作者:
and Y. Mori
中科院分区:
文献类型:
--
作者:
C. Qu;M. Yoshimura;J. Tsunoda;Y. Kaneda;M. Imade;T. Sasaki;and Y. Mori
We demonstrated a new scheme for the generation of 179 nm vacuum-ultraviolet (VUV) light with an all-solid-state laser system. It was achieved by mixing the deep-ultraviolet (DUV) of 198.8 nm and the infrared (IR) of 1799.9 nm. While CsB3O5(CBO) did not satisfy the phase-matching at around 180 nm, 179 nm output was generated with LiB3O5(LBO) for the first time. The phase-matching property of LBO at around 180 nm was also investigated. There was small deviation from theoretical curve in the measurement, which is still considered reasonable.