Oyane, A;Kawashita, M;Nakamura, T
An ethylene-vinyl alcohol copolymer (EVOH) was treated with a silane coupling agent and calcium silicate solutions, and then soaked in a simulated body fluid (SBF) with ion concentrations approximately equal to those of human blood plasma. A smooth and uniform bonelike apatite layer was successfully formed on both the EVOH plate and the EVOH-knitted fibers in SBF within 2 days. Part of the structure of the resulting apatite-EVOH fiber composite was similar to that of natural bone. If this kind of composite can be fabricated into a three-dimensional structure similar to natural bone, the resultant composite is expected to exhibit both mechanical properties analogous to those of natural bone and bone-bonding ability. Hence, it has great potential as a bone substitute. (C) 2003 Elsevier Science Ltd. All rights reserved.