Soft X-ray magnetic circular dichroism study of Al40Mn25Fe15Ge20 decagonal quasicrystal

Soft X-ray magnetic circular dichroism study of Al40Mn25Fe15Ge20 decagonal quasicrystal
复制标题

Al40Mn25Fe15Ge20十方准晶的软X射线磁圆二色性研究

DOI:
10.1016/j.nimb.2005.06.057
复制
发表时间:
2005
影响因子:
1.3
通讯作者:
K. Kobayashi
K. Kobayashi
中科院分区:
物理与天体物理4区
文献类型:
--
作者:
Tetsuya Nakamura;Y. Yokoyama;N. Kamakura;T. Matsushita;T. Hirono;T. Muro;K. Kobayashi

文献摘要

被引文献

相似文献

用软X射线磁性圆二色谱(MCD)研究了自旋玻璃Al{sub40}Mn{sub25}Fe{sub15}Ge{sub20}十方准晶(QC)的磁性。测量了元素特定磁滞回线在Mn和Fe L{sub3}边的磁滞回线随磁场强度的变化。在QC中,Mn和Fe的ESMH环有明显的差异,只有Mn环具有明显的类剩余磁化强度。ESMH的这一结果表明,在自旋玻璃QC中,Mn磁矩和Fe磁矩具有不同的磁粘性。还研究了一种铁磁性准晶Al{sub40}Mn{sub40}Ge{sub20},并与QC进行了比较。
Magnetic properties of a spin-glass Al{sub 40}Mn{sub 25}Fe{sub 15}Ge{sub 20} decagonal quasicrystal (QC) have been studied by means of soft X-ray magnetic circular dichroism (MCD). Element specific magnetic hysteresis (ESMH) loops have been measured as magnetic field dependence of MCD intensity at the Mn and Fe L{sub 3}-edges. A significant difference has been found in the ESMH loops between Mn and Fe in the QC, where only the Mn loop has an obvious remanent-like magnetization. This result of ESMH has suggested that Mn and Fe magnetic moments have different magnetic viscosities in the spin-glass QC. A ferromagnetic approximant-crystalline Al{sub 40}Mn{sub 40}Ge{sub 20} has also been investigated in comparison with the QC.