In situ studies of microstructure evolution and properties of an Al–7.5Zn–1.7Mg–1.4Cu–0.12Zr alloy during retrogression and reaging
In situ studies of microstructure evolution and properties of an Al–7.5Zn–1.7Mg–1.4Cu–0.12Zr alloy during retrogression and reaging
复制标题
Al-7.5Zn-1.7Mg-1.4Cu-0.12Zr合金回归和再时效过程中微观组织演变和性能的原位研究
DOI:
10.1016/j.matdes.2013.12.006
复制
发表时间:
2014-04
期刊:
影响因子:
--
通讯作者:
Hongwei Liu
中科院分区:
文献类型:
--
作者:
Dongmei Liu;Baiqing Xiong;Fenggang Bian;Zhihui Li;Xiwu Li;Yongan Zhang;Feng Wang;Hongwei Liu
In this work, synchrotron-based small-angle X-ray scattering technique was used for in situ tracing the evolution of microstructure parameters (including precipitate mean size, volume fraction and number density) during retrogression and reaging (RRA) treatments of an Al–7.5Zn–1.7Mg–1.4Cu–0.12Zr alloy. The mechanical and electrical properties of the alloy during RRA have also been investigated. The results show that the retrogression is characterized with a rapid dissolution stage at almost constant average precipitate size, followed by a coarsening stage with increasing precipitate size and volume fraction. The reaging treatment not only brings the re-nucleation ofη′ precipitates, but also keeps the size of the existing precipitates to a reasonable value. The developments of the mechanical and electrical properties of the alloy during RRA have been discussed based on the microstructure evolution.
登录
查看更多内容
影响因子:
8.4
作者:
Feng Wang;B. Xiong;Yongan Zhang;Zhihan Zhang;Zhixiu Wang;B. Zhu;Hongwei Liu
通讯作者:
Feng Wang;B. Xiong;Yongan Zhang;Zhihan Zhang;Zhixiu Wang;B. Zhu;Hongwei Liu
DOI:
10.1016/b978-0-12-440103-7.50009-2
发表时间:
1973
期刊:
Techniques in Protein Chemistry
影响因子:
--
作者:
Ingrid Pilz
通讯作者:
Ingrid Pilz
影响因子:
8.4
作者:
Jianbo Zhang;Yongan Zhang;B. Zhu;R. Liu;Feng Wang;Qi Liang
通讯作者:
Jianbo Zhang;Yongan Zhang;B. Zhu;R. Liu;Feng Wang;Qi Liang
DOI:
10.4028/www.scientific.net/msf.706-709.431
发表时间:
2012-01
期刊:
Materials Science Forum
影响因子:
--
作者:
B. Xiong;Xi Wu Li;Y. Zhang;Zhi Li;B. Zhu;Feng Wang;H. Liu
通讯作者:
B. Xiong;Xi Wu Li;Y. Zhang;Zhi Li;B. Zhu;Feng Wang;H. Liu
DOI:
10.1016/j.msea.2013.09.005
发表时间:
2013-12
影响因子:
6.4
作者:
Dongmei Liu;B. Xiong;Fenggang Bian;Zhi-Hui Li;Xi-wu Li;Yongan Zhang;Feng Wang;Hongwei Liu
通讯作者:
Dongmei Liu;B. Xiong;Fenggang Bian;Zhi-Hui Li;Xi-wu Li;Yongan Zhang;Feng Wang;Hongwei Liu