Thermal depolymerization of polystyrene in highly aromatic hydrocarbon medium
Thermal depolymerization of polystyrene in highly aromatic hydrocarbon medium
复制标题
DOI:
10.1016/j.jaap.2019.05.001
复制
发表时间:
2019-09-01
影响因子:
6
通讯作者:
Maksimov, Anton L.
中科院分区:
文献类型:
--
作者:
Dement'ev, Konstantin, I;Palankoev, Timur A.;Maksimov, Anton L.
Data from the thermal depolymerization of polystyrene in a highly aromatic hydrocarbon medium (light and heavy cycle oil) have been obtained. The influences of the reaction conditions on the conversion and selectivity have been studied. The maximum yield of styrene obtained in the present work is 84.4% at a polymer conversion of 93.8% in light cycle oil under the following conditions: temperature: 500 degrees C, vapor residence time: 2.61 s, polymer concentration: 15%. The styrene yield obtained is higher than has been previously reported in the scientific literature. The high selectivity of styrene in the depolymerization reaction can be explained by the fact that under the reaction conditions studied, the formation of styrene dimers in the hydrocarbon medium is inhibited.