Manufacture by selective laser melting and mechanical behavior of a biomedical Ti–24Nb–4Zr–8Sn alloy
Manufacture by selective laser melting and mechanical behavior of a biomedical Ti–24Nb–4Zr–8Sn alloy
复制标题
DOI:
10.1016/j.scriptamat.2011.03.024
复制
发表时间:
2011-06
影响因子:
6
通讯作者:
Lai‐Chang Zhang;D. Klemm;J. Eckert;Y. Hao;T. Sercombe
中科院分区:
文献类型:
--
作者:
Lai‐Chang Zhang;D. Klemm;J. Eckert;Y. Hao;T. Sercombe
In this paper, we present the results of using selective laser melting (SLM) to produce biomedical beta Ti–24Nb–4Zr–8Sn components, including the manufacture of a sample acetabular cup. The density of the material increases with increasing incident laser energy (i.e. decreasing laser scan speed) and reaches a near full density value of >99% without any post-processing. The mechanical properties of the as-processed material are also compared to those of conventionally processed material.