I. DELAYED THERMAL CONTRACTION AND CRAZING OF CERAMIC GLAZES

I. DELAYED THERMAL CONTRACTION AND CRAZING OF CERAMIC GLAZES
复制标题

DOI:
10.1111/j.1151-2916.1946.tb11580.x
复制
发表时间:
1946-07
影响因子:
3.9
通讯作者:
L. Mattyasovszky-Zsolnay
L. Mattyasovszky-Zsolnay
中科院分区:
材料科学2区
文献类型:
--
作者:
L. Mattyasovszky-Zsolnay

文献摘要

被引文献

相似文献

实验棒,釉面与16种不同的釉,代表各种可能类型的陶器釉,在Steger应力测量仪进行了测试之前和之后的五年密闭储存。所有釉料的初始应力在该方法的准确度范围内保持恒定,表明釉料的延迟热收缩可以忽略不计。
Experimental rods, glazed with sixteen different glazes, representing various possible types of earthenware glazes, were tested in the Steger stress-measuring apparatus before and after five years of airtight storage. The original stress of all the glazes remained constant within the limit of accuracy of the method, indicating that the delayed thermal contraction of the glazes is negligible.