Quick Response of All Solid Electrochromic Device
Quick Response of All Solid Electrochromic Device
复制标题
全固体电致变色器件的快速响应
DOI:
10.1143/apex.2.105502
复制
发表时间:
2009
影响因子:
2.3
通讯作者:
Y. Moritomo
中科院分区:
文献类型:
--
作者:
T. Shibata;Y. Moritomo
We fabricated all solid electrochromic devices by connecting two kinds of cyanide thin films. We found that the magnitude of tR decreases with increase in the electric pressure |V| as tR∝|V|-1 and with decrease in the device thickness dD as tR∝(dD-2dEDL)2, where dEDL (=50–100 nm) is the effective thickness of the electric double layer (EDL). These observations are well understood in terms of the leaked electric pressure from the EDL region, perhaps originated in the imperfect screening of V.
DOI:
--
发表时间:
2008
期刊:
J. Phys. Soc. Jpn 77
影响因子:
--
作者:
T. Shibata;F. Nakata;H. Kamioka and Y. Moritomo
通讯作者:
H. Kamioka and Y. Moritomo