Giant negative thermal expansion in Fe-doped layered ruthenate ceramics
Giant negative thermal expansion in Fe-doped layered ruthenate ceramics
复制标题
DOI:
10.7567/apex.10.115501
复制
发表时间:
2017-11-01
影响因子:
2.3
通讯作者:
Azuma, Masaki
中科院分区:
文献类型:
--
作者:
Takenaka, Koshi;Shinoda, Tsubasa;Azuma, Masaki
The effects of iron doping on the giant negative thermal expansion (NTE) of Ca2RuO4-y ceramics are investigated. Fe-doped ruthenate ceramics exhibit a large NTE even though the crystallographic unit-cell volume shows no NTE. The anisotropic thermal strain of crystal grains consumes open spaces in the sintered body and causes giant bulk volume contraction on heating. This giant NTE is reproducible against repeated thermal cycling, indicating a tough microstructure. The thermal expansion of epoxy resin is fully suppressed below 400K by the 56 vol% loading of the Fe-doped ruthenate ceramic powder, demonstrating tough microstructures and the capability of thermal expansion compensation of the ruthenate sintered body. (C) 2017 The Japan Society of Applied Physics