Controllable fabrication and properties of polypropylene nanofibers

Controllable fabrication and properties of polypropylene nanofibers
复制标题

DOI:
10.1002/pen.20896
复制
发表时间:
2007-11
影响因子:
3.2
通讯作者:
Dong Wang;Gang Sun;B. Chiou;J. Hinestroza
Dong Wang;Gang Sun;B. Chiou;J. Hinestroza
中科院分区:
工程技术4区
文献类型:
--
作者:
Dong Wang;Gang Sun;B. Chiou;J. Hinestroza

文献摘要

被引文献

相似文献

Thermoplastic nanofibers in yarn form were prepared by melt extrusion of immiscible blends of cellulose acetate butyrate (CAB) and thermoplastic polymers and subsequent removal of the CAB matrix. Isotactic polypropylene (iPP) nanofiber, with diameters ranging from 75 to 375 nm, were made by using CAB/iPP blends, with a ratio of 97.5–2.5, and a hot-drawn ratio of 25 in a twin-screw extruder. Dispersion of iPP in CAB and shear and elongational deformation are major factors to result in nanosized fibers. The spheres and nanofibers with different diameters of iPP dispersed phases in the CAB matrix can be well controlled by changing the flow field and the blend ratio. Differential scanning calorimeter and wide angle X-ray diffraction results showed that the nanofibers had lower crystallinity and crystallite thickness compared with bulk iPP. The atomic force microscopy images presented the well-defined nanofiber morphology and the excellent manipulability of single iPP nanofiber separated from a bundle of iPP nanofibers. POLYM. ENG. SCI., 47:1865–1872, 2007. © 2007 Society of Plastics Engineers