用透射电镜研究了彩色阴极射线管荫罩用Fe-36%Ni因瓦合金的再结晶行为和晶粒长大。r值随着(111)表面强度的增加而增加。在轻冷轧压下量的情况下,退火后再结晶组织的核心取向为(011),并且核心被(011)取向的冷轧基体包围。另一方面,在大冷轧压下量的情况下,退火后再结晶组织的核取向为(011)和(100)。这两个核心被相同的冷轧矩阵的(011)取向与轻冷轧压下量包围。
Recrystallization behavior and grain growth in Fe-36%Ni invar alloy for shadow masks in color cathode ray tubes are studied by using transmission electron microscopy. The r-value increases with increasing (111) surface intensity. In case of light cold-rolling reduction, nuclei orientations of recrystallized structure after annealing are (011) and the nuclei are surrounded by cold rolled matrices of (011) orientation. On the other hand, in case of heavy cold rolling reduction, nuclei orientations of recrystallized structure after annealing are (011) and (100). These two nuclei are surrounded by the same cold rolled matrices of (011) orientation with light cold rolling reduction.