Preparation of Yttria-Stabilized Zirconia Films for Solid Oxide Fuel Cells by Electrophoretic Deposition Method.

Preparation of Yttria-Stabilized Zirconia Films for Solid Oxide Fuel Cells by Electrophoretic Deposition Method.
复制标题

电泳沉积法制备固体氧化物燃料电池用氧化钇稳定氧化锆薄膜。

DOI:
10.1246/cl.1992.943
复制
发表时间:
1992
期刊:
影响因子:
--
通讯作者:
Y. Takita
Y. Takita
中科院分区:
--
文献类型:
--
作者:
T. Ishihara;Keiji Sato;Y. Mizuhara;Y. Takita

文献摘要

被引文献

相似文献

采用电泳沉积(EPD)方法制备用于固体氧化物燃料电池(SOFC)的氧化钇稳定氧化锆(YSZ)薄膜。 EPD方法可以很容易地制备厚度均匀的致密YSZ薄膜。当使用La0.6Sr0.4MnO3作为阴极、化学镀Pt作为阳极制备平面SOFC时,开路电压和最大功率密度分别为1.03 V和1.87 Wcm−2。
The electrophoretic deposition (EPD) method was applied for the preparation of yttria-stabilized zirconia (YSZ) films for a solid oxide fuel cell (SOFC). Dense YSZ films with uniform thickness can be readily prepared by EPD method. When the planar SOFC was fabricated by using La0.6Sr0.4MnO3 as a cathode and electroless plating Pt as an anode, the open circuit voltage and the maximum power density attained were 1.03 V and 1.87 Wcm−2, respectively.