Crack resistance of fiber-reinforced asphalt mixtures: Effect of test specimen and test condition
Crack resistance of fiber-reinforced asphalt mixtures: Effect of test specimen and test condition
复制标题
DOI:
10.1111/ffe.13647
复制
发表时间:
2022-01-17
影响因子:
3.7
通讯作者:
Haghighatpour, Pegah Jafari
中科院分区:
文献类型:
--
作者:
Hajiloo, Hamid Reza;Karimi, Hamid Reza;Haghighatpour, Pegah Jafari
The effect of some important testing conditions including test specimen (SCB and ENDB), fracture mode (I and II), loading rate (0.5, 1.0, and 5.0 mm/min), and temperature (-5 degrees C, -15 degrees C, and -25 degrees C) is evaluated on fracture toughness of asphalt material containing different percentages of fibers (0%, 0.025%, 0.05%, and 0.1% of unit weight). The experimental and numerical results show that the addition of 0.025%, 0.05%, and 0.1% of the polyolefin-aramid fiber in asphalt mixture increases the fracture toughness of the control mixture by about 8%, 17%, and 23% in pure mode I and 7%, 16%, and 24% in pure mode II, respectively; which are among the most promising enhancements compared to other fibers. Results also reveal that fracture toughness at mode I obtained from the SCB and ENDB specimens is similar. However, the mode II fracture toughness obtained from the ENDB specimen is about 12% higher than the corresponding value obtained from the SCB specimen.