Single crystals of the ferroelectric mixed Aurivillius phase Bi7Ti4NbO21have been prepared by the flux method in Bi2O3excess. Thermal dependence of dielectric permittivity, X-ray diffraction patterns, birefringence and optical observations as well as differential scanning calorimetry have been studied between room temperature and 900 °C. Two temperature driven phase transitions were observed, the first one close to 630–675 °C within a ferroelectric state (ferro I-ferro II), the second one at ≈ 830 °C, between the ferroelectric state II and the paraelectric state.