Microstructure and deformation behavior of Ti-10V-2Fe-3Al alloy during hot forming process

Microstructure and deformation behavior of Ti-10V-2Fe-3Al alloy during hot forming process
复制标题

Ti-10V-2Fe-3Al合金热成形过程中的显微组织及变形行为

DOI:
10.1007/s11595-015-1317-0
复制
发表时间:
2015-12
期刊:
Journal of Wuhan University of Technology Materials Science
影响因子:
--
通讯作者:
Lee C. S.
Lee C. S.
中科院分区:
其他
文献类型:
--
作者:
Guan R. G.;Zhao Z. Y.;Choi K. S.;Lee C. S.

文献摘要

参考文献

相似文献

研究了Ti-10 V-2Fe-3Al合金在热成形过程中的组织演变和成形性能与初始组织和工艺参数的关系。实验结果表明,α相的生长受固溶体的控制
The microstructure evolution and formability of Ti-10V-2Fe-3Al alloy related to the initial microstructures and processing variables were investigated during hot forming process. The experimental results show that the α-phase growth is controlled by solut
DOI: 10.1179/mst.1997.13.7.575
发表时间: 1997-07
影响因子: 1.8
作者:
D. Robertson;H. Mcshane
通讯作者: D. Robertson;H. Mcshane
DOI: 10.1361/105994905x75448
发表时间: 2005-12-01
影响因子: 2.3
作者:
Boyer, RR;Briggs, RD
通讯作者: Briggs, RD
DOI: 10.1007/s11661-001-0155-1
发表时间: 2001-07-01
影响因子: 2.8
作者:
Semiatin, SL;Bieler, TR
通讯作者: Bieler, TR
DOI: 10.1016/j.msea.2008.09.071
发表时间: 2009-02-15
影响因子: 6.4
作者:
Jackson, M.;Jones, N. G.;Dashwood, R. J.
通讯作者: Dashwood, R. J.
DOI: 10.1023/a:1012972509205
发表时间: 2001-12
影响因子: 4.5
作者:
Y. Wu;S. Hwang
通讯作者: Y. Wu;S. Hwang