SiC coating toughened by HfC nanowires to protect C/C composites against oxidation
SiC coating toughened by HfC nanowires to protect C/C composites against oxidation
复制标题
HfC 纳米线增韧的 SiC 涂层可保护 C/C 复合材料免受氧化
DOI:
10.1016/j.apsusc.2014.05.042
复制
发表时间:
2014-08
影响因子:
6.7
通讯作者:
Zhixiong Hu
中科院分区:
文献类型:
--
作者:
Jincui Ren;Song Tian;Hejun Li;Zhixiong Hu
To prevent carbon/carbon (C/C) composites from oxidation at high temperature, a dense SiC coating toughened by HfC nanowires was prepared by a two-step technique of chemical vapor deposition (CVD) and pack cementation. The microstructure, mechanical properties and oxidation resistance of the coating were investigated. The HfC nanowires can effectively reduce the size of microcracks and avoid the formation of through-thickness microcracks in the SiC coating. Due to the toughening mechanisms including microcrack bridging by nanowire and nanowire pullout, the mechanical properties and oxidation resistance of the coating are improved.
登录
查看更多内容
影响因子:
1.8
作者:
Shouyang Zhang;Yongjie Wang;Jincui Ren;Xinfa Qiang
通讯作者:
Xinfa Qiang
影响因子:
10.9
作者:
Xiaohong Shi;Hejun Li;Q. Fu;Jinhua Lu;Kezhi Li
通讯作者:
Xiaohong Shi;Hejun Li;Q. Fu;Jinhua Lu;Kezhi Li
影响因子:
10.9
作者:
Jacobson, NS;Curry, DM
通讯作者:
Curry, DM
影响因子:
6.7
作者:
Yongjie Wang;Hejun Li;Q. Fu;Heng Wu;Dong-jia Yao;B. Wei
通讯作者:
Yongjie Wang;Hejun Li;Q. Fu;Heng Wu;Dong-jia Yao;B. Wei
DOI:
10.1016/s0955-2219(98)00242-8
发表时间:
1997-04
期刊:
Key Engineering Materials
影响因子:
--
作者:
H. Fritze;J. Jojic;T. Witke;C. Rüscher;S. Weber;S. Scherrer;B. Schultrich;G. Borchardt
通讯作者:
H. Fritze;J. Jojic;T. Witke;C. Rüscher;S. Weber;S. Scherrer;B. Schultrich;G. Borchardt