Protium absorption properties of La-Tm-Si (TM=Co, Ni) ternary intermetallic compounds
Protium absorption properties of La-Tm-Si (TM=Co, Ni) ternary intermetallic compounds
复制标题
La-Tm-Si (TM=Co, Ni)三元金属间化合物的氕吸收性能
DOI:
10.2320/matertrans1989.39.769
复制
发表时间:
1998
期刊:
影响因子:
--
通讯作者:
M. Okada
中科院分区:
文献类型:
--
作者:
H. Kakuta;Toshiyuki Ogawa;H. Takamura;M. Okada
The protium-absorbing characteristics such as the amount of absorbing protium and the hydrogen reaction have been studied for the LaTMSi, LaTMSi 2 and LaTM 2 Si 2 (TM=Co, Ni) ternary intermetallic compounds. For these compounds, it is found from DSC measurements that only the LaCoSi and LaNiSi compounds show hydride reactions at elevated temperatures. The LaCoSi alloy has a disproportionation reaction at 457 K, whereas the LaNiSi alloy reversibly absorbs and desorbs protium near 425 K. The maximum absorbed amount of protium is 0.52 mass% for the LaNiSi alloy.