Reduced electronegativity difference as a factor leading to the formation of Al-based glassy alloys with a large supercooled liquid region of 50K
Reduced electronegativity difference as a factor leading to the formation of Al-based glassy alloys with a large supercooled liquid region of 50K
复制标题
DOI:
10.1063/1.2159420
复制
发表时间:
2006-01
影响因子:
4
通讯作者:
D. V. Louzguine-Luzgin;A. Inoue;W. Botta
中科院分区:
文献类型:
--
作者:
D. V. Louzguine-Luzgin;A. Inoue;W. Botta
The influence of the electronegativity difference among the constituent elements on the stability of the supercooled liquid in two Al-based glassy alloys is studied. A record-large value of the supercooled liquid region of about 50K is obtained based on the electronegativity difference concept within a certain composition range.