Recent Advances in Self‐Healing Materials Systems
Recent Advances in Self‐Healing Materials Systems
复制标题
自修复材料系统的最新进展
DOI:
10.1002/9780470512067.ch9
复制
发表时间:
2007
期刊:
影响因子:
--
通讯作者:
N. Sottos
中科院分区:
文献类型:
--
作者:
M. W. Keller;B. Blaiszik;S. White;N. Sottos
Damage in polymeric coatings, adhesives, microelectronic components and structural composites can span many length scales. Some common examples of crack damage and the corresponding length scales are summarized in Figure 9.1. Structural composites subject to impact loading can sustain significant damage on the order of tens of centimeters, which in turn can lead to subsurface millimeter-scale delaminations and micron-scale matrix cracking