On the onset of fracture as a silicon‐based polymer converts into the ceramic phase
On the onset of fracture as a silicon‐based polymer converts into the ceramic phase
复制标题
当硅基聚合物转变为陶瓷相时断裂开始
DOI:
10.1111/jace.16089
复制
发表时间:
2018
影响因子:
3.9
通讯作者:
Soraru, Gian Domenico
中科院分区:
文献类型:
--
作者:
Raj, Rishi;Pederiva, Luca;Narisawa, Masaki;Soraru, Gian Domenico
Silicon‐based polymers evolve into refractory ceramics when heated gradually up to ~1000°C. The conversion is accompanied by the loss of gaseous species, and by a two‐fold increase in density. The shrinkage can produce microcracks if the heating rate is too high, or if the specimen is too thick. This communication builds on earlier work whereby the measurement of gas evolution, and its relationship with viscous flow, are related to the onset of fracture in disk‐shaped green (polymer) samples. The onset is determined as a function of the thickness of the disks, and of the heating rate. The results are presented in the form of a processing map. The overlay with gas evolution, and strain‐rate measurements, suggest that fracture initiates with the release of hydrogen and methane, starting at temperatures near 750°C.
DOI:
--
发表时间:
1994
期刊:
影响因子:
--
作者:
K. L. Edwards
通讯作者:
K. L. Edwards
DOI:
--
发表时间:
2012
期刊:
影响因子:
--
作者:
G. Sorarù;A. Karakuscu;C. Boissière;F. Babonneau
通讯作者:
F. Babonneau