Preparation of 0.83(Bi0.5Na0.5)TiO3-0.17BaTiO3 thick films by screen printing
Preparation of 0.83(Bi0.5Na0.5)TiO3-0.17BaTiO3 thick films by screen printing
复制标题
丝网印刷法制备0.83(Bi0.5Na0.5)TiO3-0.17BaTiO3厚膜
DOI:
10.7567/jjap.56.10pf01
复制
发表时间:
2017
影响因子:
1.5
通讯作者:
Y. Sakai and T. Karaki
中科院分区:
文献类型:
--
作者:
Ishibashi;T.;榮野川優也,小野尋子;石橋俊之;石橋俊之;石橋俊之;Y. Sakai and T. Karaki