Hydrogenation of the wide-gap oxide semiconductor as a room-temperature and 3D-compatible electron doping technique
Hydrogenation of the wide-gap oxide semiconductor as a room-temperature and 3D-compatible electron doping technique
复制标题
宽禁带氧化物半导体的氢化作为室温和 3D 兼容的电子掺杂技术
DOI:
10.1063/1.5055302
复制
发表时间:
2018
期刊:
影响因子:
1.6
通讯作者:
Toriumi A.
中科院分区:
文献类型:
--
作者:
Yajima T.;Oike G.;Yamaguchi S.;Miyoshi S.;Nishimura T.;Toriumi A.