高质量的六方相中孔二氧化硅纤维(见图)可以通过本文报道的一步两相室温合成的一般程序生长。该二氧化硅纤维直径为1-5 μ m,长度可达5cm,具有优良的长程有序性,窄的孔径分布和高达0.78cm(3)/g的孔体积。双折射光纤可用作高表面积光纤。
High-quality, hexagonal phase, mesoporous silica fibers (see Figure) can be grown by the general procedure for one-step, two-phase, room temperature synthesis reported here. The silica fibers, which are 1-5 mu m in diameter and up to 5 cm long, have excellent long-range order, a narrow pore size distribution, and a pore volume of up to 0.78 cm(3)/g. The birefringent fibers can be used as high-surface-area optical fibers.