Room‐temperature preparation of crystallized luminescent Sr1−xCaxWO4 solid‐solution films by an electrochemical method
Room‐temperature preparation of crystallized luminescent Sr1−xCaxWO4 solid‐solution films by an electrochemical method
复制标题
电化学方法室温制备结晶发光Sr1−xCaxWO4固溶体薄膜
DOI:
10.1063/1.116781
复制
发表时间:
1996
影响因子:
4
通讯作者:
M. Yoshimura
中科院分区:
文献类型:
--
作者:
Woo;M. Yashima;M. Kakihana;A. Kudo;T. Sakata;M. Yoshimura
A complete series of well‐crystallized solid‐solution oxide films, Sr1−XCaXWO4 (0≤X≤1), has been prepared on a tungsten substrate in the electrolytic solution containing Sr2+ and Ca2+ ions by an electrochemical method at room temperature (25 °C). The composition of solid‐solution oxide films could easily be controlled by the concentrations of Sr and Ca species in the starting solutions. The films showed only single blue emission at liquid nitrogen temperature (−196 °C), strongly suggesting that they consisted of well‐crystallized defect‐free crystals.