Study on deactivation of Ni/Al2O3 catalyst for liquid phase hydrogenation of crude 1,4-butanediol aqueous solution

Study on deactivation of Ni/Al2O3 catalyst for liquid phase hydrogenation of crude 1,4-butanediol aqueous solution
复制标题

粗1,4-丁二醇水溶液液相加氢Ni/Al2O3催化剂失活研究

DOI:
10.1016/j.cej.2011.06.029
复制
发表时间:
2012-02-01
影响因子:
15.1
通讯作者:
Liang, Xiaoyuan
Liang, Xiaoyuan
中科院分区:
工程技术1区
文献类型:
--
作者:
Li, Haitao;Zhao, Yongxiang;Liang, Xiaoyuan

文献摘要

被引文献

相似文献

The deactivation of a commercial Ni/Al2O3 catalyst in the liquid phase hydrogenation of crude 1,4-butanediol aqueous solution was investigated. A significant deactivation trend was observed during the operation time of 5000 h. The fresh and deactivated catalysts were characterized by ICP-AES, N-2 physisorption, H-2-TPR, TEM, TPD, FTIR and XRD. The results indicate that, during the reaction process, the Al2O3 support transforms into its hydrate boehmite (gamma-AlO(OH)), which further results in the aggregation of metal Ni, the decrease of BET specific surface area and the reduction of pore volume. The hydration of Al2O3 support is the main reason for the deactivation of Ni/Al2O3 catalyst. The promotion effect of SiO2 on the activity and stability of Ni/Al2O3 catalyst was also investigated. The results suggest that the introduction of SiO2 effectively inhibits the hydration of Al2O3 support and prevents the active decay of Ni/Al2O3 catalyst. (C) 2011 Elsevier B.V. All rights reserved.