Recovery Uranium from Uranium-Bearing Waste Ore Using Heap Bioleaching

Recovery Uranium from Uranium-Bearing Waste Ore Using Heap Bioleaching
复制标题

DOI:
10.4028/www.scientific.net/amr.518-523.3187
复制
发表时间:
2012-05
期刊:
Advanced Materials Research
影响因子:
--
通讯作者:
Xue Gang Wang;Z. Zheng;Zhanxue Sun;Ya Jie Liu
Xue Gang Wang;Z. Zheng;Zhanxue Sun;Ya Jie Liu
中科院分区:
其他
文献类型:
--
作者:
Xue Gang Wang;Z. Zheng;Zhanxue Sun;Ya Jie Liu

文献摘要

被引文献

相似文献

研究了从中国南部某铀矿床含铀废矿中堆浸回收铀的可行性。在废矿场建设了一个4500吨的工业堆。废矿样粉碎至-25 mm,矿石铀品位为0.0211%。生产146d后,渣铀浸出率为55.92%,渣中铀含量为0.0093%,酸耗为2.69%(以矿重计)。研究证明,用堆浸方法从含铀废矿中回收铀是可行的。
The feasibility of heap bioleaching recovery of uranium from the one Uranium Mine deposit uranium-bearing waste ore, located in south of China, were investigated. A 4500 ton industrial heap was constructed in the waste ore dump site. The waste ore sample was crushed to -25 mm, the ore uranium grade is 0.0211%. After 146 days of performance, the slag uranium leaching rate was 55.92% that calculated by its residue has been recovered, content of uranium in residue was 0.0093%, the acid consumption rate was 2.69% by ore weight. The study has proven that recovery uranium from uranium-bearing waste ore using heap bioleaching is feasible.