Effects of Cl on the reduction of supported PdO in ethanol/water solvent mixtures

Effects of Cl on the reduction of supported PdO in ethanol/water solvent mixtures
复制标题

Cl 对乙醇/水溶剂混合物中负载型 PdO 还原的影响

DOI:
10.1080/2055074x.2016.1267296
复制
发表时间:
2017
期刊:
Catalysis, Structure & Reactivity
影响因子:
--
通讯作者:
Brazier J
Brazier J
中科院分区:
--
文献类型:
--
作者:
Brazier J

文献摘要

参考文献

被引文献

相似文献

研究了γ-Al_2O_3负载PdO在流动乙醇水溶液中的还原反应。快速EXAFS(QEXAFS)在Pd K-边缘进行表明,Cl的存在下,可以有一个深刻的影响的还原过程。在低负载量的Pd(1重量%),该过程的尺寸依赖性是相反的,相比无Cl样品。发现减少的程度取决于负载/颗粒尺寸。它表明,usingin situQEXAFS在Cl的K-和Pd的L3-边缘,残留的Cl不被除去的流动的溶剂混合物,即使在350 K的高温。这些行为的起源进行了讨论,在不同的影响,Cl可能有键合到氧化或还原的金属中心和结果进行了比较,对商业聚脲封装的Pd ENCAT™ NP 30催化剂上的Cl的影响的早期观察。
The reduction of γ-Al2O3-supported PdO in flowing aqueous ethanol was investigated. Quick EXAFS (QEXAFS) performed at the Pd K-edge reveals that the presence of Cl can have a profound effect on the reduction process. At low loadings of Pd (1 wt-%), the size dependency of the process is inverted, compared to Cl-free samples. The extent of reduction was found to be dependent on loading/particles size. It is shown, usingin situQEXAFS at the Cl K- and Pd L3-edges, that residual Cl is not removed by the flowing solvent mixture, even at an elevated temperature of 350 K. The origins of these behaviours are discussed in terms of the differing effects that Cl may have when bonded to oxidic or reduced metal centres and the results were compared to earlier observations made on the effects of Cl on commercial polyurea encapsulated Pd ENCAT™ NP 30 catalysts.
DOI: --
发表时间: 1995
期刊:
影响因子: --
作者:
S. Shadle;B. Hedman;K. Hodgson;E. Solomon
通讯作者: E. Solomon
DOI: --
发表时间: 1970
期刊:
影响因子: --
作者:
S. Nakamura;T. Yasui
通讯作者: T. Yasui
DOI: --
发表时间: 1975
期刊:
影响因子: --
作者:
R. Duś
通讯作者: R. Duś
有机金属衍生的 Pd/MgO 催化剂上 CO 化学吸附的 DRIFT 研究:氯的影响
DOI: --
发表时间: 1996
期刊:
影响因子: --
作者:
M. Kappers;C. Dossi;R. Psaro;S. Recchia;A. Fusi
通讯作者: A. Fusi
Pd/γ-Al2O3 上的新戊烷转化
DOI: --
发表时间: 1995
期刊:
影响因子: --
作者:
W. Juszczyk;D. Lomot;Z. Karpiński;J. Pielaszek
通讯作者: J. Pielaszek