Cuprous oxide nanowires prepared by an additive-free polyol process

Cuprous oxide nanowires prepared by an additive-free polyol process
复制标题

DOI:
10.1021/cg060615t
复制
发表时间:
2007-02-01
影响因子:
3.8
通讯作者:
Zigon, Majda
Zigon, Majda
中科院分区:
化学2区
文献类型:
--
作者:
Orel, Zorica Crnjak;Anzlovar, Alojz;Zigon, Majda

文献摘要

被引文献

相似文献

首次采用多元醇法制备了氧化亚铜纳米线,其前驱体为一水乙酸铜和二甘醇(DEG)。在控制反应温度(190℃)、前驱体浓度(0.01 ~ 0.1 mol/L)和反应时间(6 h)的条件下,制备了直径约为20 nm、长度可达5 μ m的Cu2O纳米线,并用SEM、TEM、XRD和IR对其进行了表征。
The polyol method was employed for the first time to synthesize cuprous oxide nanowires using only a precursor of Cu(II) acetate monohydrate and diethylene glycol (DEG). With careful control of the reaction temperature (190 degrees C), the precursor concentration (0.01-0.1 mol/L), and the reaction time (6 h), we prepared Cu2O nanowires with a diameter of approximately 20 nm and a length up to 5 mu m. The nanowires were characterized by SEM, TEM, XRD, and IR spectroscopy.