Solid state phase transformations in LiAlH4 during high-energy ball-milling
Solid state phase transformations in LiAlH4 during high-energy ball-milling
复制标题
DOI:
10.1016/s0925-8388(00)01201-9
复制
发表时间:
2000-12-15
影响因子:
6.2
通讯作者:
Dennis, KW
中科院分区:
文献类型:
--
作者:
Balema, VP;Pecharsky, VK;Dennis, KW
Mechanochemical processing of polycrystalline LiAlH4 revealed good stability of this complex aluminohydride during high-energy ball-milling in a helium atmosphere for up to 35 h. The decomposition of lithium aluminohydride into Li3AlH6, Al and H-2 is observed during prolonged mechanochemical treatment for up to 110 h and is most likely associated with the catalytic effect of a vial material, iron, which is introduced into the hydride as a contaminant during mechanical treatment. (C) 2000 Elsevier Science B.V. All rights reserved.