将二氧化硅碳热还原成硅需要使用远高于硅熔点 (>= 2,000 摄氏度)(1) 的温度。最近,固体硅是在低得多的温度(500 m(2) g(-1))下直接由二氧化硅生成的,并且含有大量的微孔(
The carbothermal reduction of silica into silicon requires the use of temperatures well above the silicon melting point (>= 2,000 degrees C)(1). Solid silicon has recently been generated directly from silica at much lower temperatures (500 m(2) g(-1)), and contained a significant population of micropores (