Extension of Measurements of the Tensile Flow Stress of High-Purity α-Iron Single Crystals to Very Low Temperatures
Extension of Measurements of the Tensile Flow Stress of High-Purity α-Iron Single Crystals to Very Low Temperatures
复制标题
将高纯 α-铁单晶拉伸流动应力的测量扩展到极低温度
DOI:
--
复制
发表时间:
1992
期刊:
影响因子:
--
通讯作者:
J. Diehl
中科院分区:
文献类型:
--
作者:
D. Brunner;J. Diehl
Measurements on the flow stress of high-purity α-Fe single crystals, carried out by successive tensile deformation steps at different temperatures and combined with stress-relaxation tests, were extended to about 4 K. The temperature dependence of the flow stress down to the lowest temperatures can be described very well by Seeger's theory of kink-pair formation in screw dislocations and an Arrhenius equation with an almost constant preexponential factor