The effect of time on optical coating mechanical loss and implications for LIGO-India
The effect of time on optical coating mechanical loss and implications for LIGO-India
复制标题
时间对光学镀膜机械损耗的影响及其对 LIGO-India 的影响
DOI:
10.1088/0264-9381/33/14/147001
复制
发表时间:
2016
影响因子:
3.5
通讯作者:
S. Penn
中科院分区:
文献类型:
--
作者:
M. Kinley;H. Fair;Isaac Jiffar;Jonathan Newport;L. Gitelman;G. Harry;G. Billingsley;S. Penn
We report on the persistence of mechanical loss with time of ion beam sputtered dielectric coatings made from alternating layers of Ta2O5 and SiO2 deposited onto fused silica substrates. From this, we predict the coating thermal noise in gravitational wave interferometers, after the coated optics have been stored for years. We measured the modal mechanical quality factor, Q, of two coated fused silica samples in 2015. These samples also had their modal Q's measured in 2002. We conclude that storing the coated silica disks for 13 years does not change their mechanical loss and thus the storage of Advanced LIGO gravitational wave detector optics until their future installation in India will not degrade their achievable thermal noise.