Adsorption deformation of a microporous AR-V carbon adsorbent during the adsorption of benzene

Adsorption deformation of a microporous AR-V carbon adsorbent during the adsorption of benzene
复制标题

微孔AR-V碳吸附剂吸附苯过程中的吸附变形

DOI:
10.1134/s2070205112040120
复制
发表时间:
2012
影响因子:
1.1
通讯作者:
A. V. Tvardovskii
A. V. Tvardovskii
中科院分区:
材料科学4区
文献类型:
--
作者:
V. V. Nabiulin;A. Fomkin;A. V. Tvardovskii

文献摘要

被引文献

相似文献

测定了AR-V微孔碳吸附剂在1 Pa ~ 14 kPa压力范围和255 ~ 353 K温度范围内对苯的吸附等温线和吸附引起的变形。在低压区,在333和353 K温度下,AR-V吸附剂发生收缩,随着压力的增加,收缩变为膨胀。在低温区(255-313 K),在整个研究压力范围内,只观察到AR-V吸附剂的膨胀。吸附剂的最大相对压缩值在0.18% ~ 0.08%之间变化,对应温度在353 ~ 333 K之间变化。随着相应温度从293 ~ 353 K的升高,最大相对膨胀率从0.9 ~ 0.05%变化。
Adsorption isotherms of benzene and adsorption-induced deformation of the AR-V microporous carbon adsorbent in the pressure range from 1 Pa to 14 kPa and at temperatures from 255 to 353 K have been determined. Contraction of the AR-V adsorbent is observed at temperatures of 333 and 353 K in the lowpressure area, which changes into expansion with an increase in pressure. In a low-temperature area (255–313 K), only expansion of the AR-V adsorbent is observed in the whole range of the studied pressures. The value of the maximal relative compression of the adsorbent changes from 0.18 to 0.08%, while the corresponding temperature varies from 353 to 333 K. The maximal relative expansion changes from 0.9 to 0.05% along with an increase in the corresponding temperature from 293 to 353 K.