铁磁大块非晶合金Fe 40 Ni 40 P 14 B6。可以通过快速淬火技术制备直径接近1.2mm的棒。如果还使用助熔技术,则可以合成直径大至类似于2.5mm的非晶棒。Fe_(40)Ni_(40)P_(14)B_6玻璃形成的临界冷却速率R_c约为10(2)K·s ~(-1)。(c)2006 Elsevier B. V.保留所有权利。
Ferromagnetic bulk amorphous Fe40Ni40P14B6 alloy. rods with a diameter of similar to 1.2mm can be prepared by means of a rapid quenching technique. If a fluxing technique is also used, amorphous rods with a diameter as large as similar to 2.5 mm can be synthesized. The critical cooling rate R-c for the glass formation Fe40Ni40P14B6 is estimated to-be on the order of 10(2)K s(-1). (c) 2006 Elsevier B.V. All rights reserved.