Tensile creep behavior of 3-D woven Si-Ti-C-O fiber/SiC-based matrix composite with glass sealant
Tensile creep behavior of 3-D woven Si-Ti-C-O fiber/SiC-based matrix composite with glass sealant
复制标题
玻璃密封胶 3D 编织 Si-Ti-C-O 纤维/SiC 基复合材料的拉伸蠕变行为
DOI:
10.1023/a:1004796615811
复制
发表时间:
2000
影响因子:
4.5
通讯作者:
T. Hirokawa
中科院分区:
文献类型:
--
作者:
T. Ogasawara;T. Ishikawa;N. Suzuki;I. Davies;M. Suzuki;J. Gotoh;T. Hirokawa
The present work investigates the tensile creep behavior (deformation and rupture) at 1100–1300°C in air of a 3-D woven Si-Ti-C-O (Tyranno™) fiber/SiC-based matrix composite with and without glass sealant. The composite contained Si-Ti-C-O fibers with an additional surface modification in order to improve interface properties. Although a significant decrease in tensile strength was observed in the unsealed composite beyond 1000°C in air (and attributed to oxidation of the fiber/matrix interface), the composite with glass sealant possessed excellent mechanical properties for short-term (<1 hr.) exposure in air. In this study, tensile creep testing was conducted at 1100–1300°C in air and the effect of glass sealant on medium- and long-term strength was investigated. In addition, chemical stability of the glass sealant was evaluated by X-ray diffraction analysis (XRD) and energy dispersive X-ray spectrometer (EDS). The creep rupture behavior of the composite with glass sealant under long-term exposure is suggested to depend on several factors including decomposition, evaporation, and crystallization of the glass sealant material, in addition to the applied stress.