Non-destructive Measurement of Residual Stress Depth Profile in Laser-peened Steel at SPring-8
Non-destructive Measurement of Residual Stress Depth Profile in Laser-peened Steel at SPring-8
复制标题
SPring-8 激光喷丸钢残余应力深度轮廓的无损测量
DOI:
10.1063/1.2436367
复制
发表时间:
2007
影响因子:
0.5
通讯作者:
K. Akita
中科院分区:
文献类型:
--
作者:
Masugu Sato;Y. Sano;K. Kajiwara;Hirotomo Tanaka;K. Akita
We investigated the residual stress depth profile near the surface of steel treated by laser peening without coating using X‐ray diffraction at SPring‐8. This investigation was carried out using a constant penetration depth sin2ψ method. In this method, the sin2ψ diagram is measured controlling both the ψ angle and the X‐ray penetration depth simultaneously with a combination of the ω and χ axes of the 4‐circle goniometer. This method makes it possible to evaluate the residual stress and its depth profile in material with a stress gradient precisely and non‐destructively. As a result, we confirmed that a compressive residual stress was successfully formed all over the range of the depth profile in the steel treated properly by laser peening without coating.