Preparation of pressureless-sintered SiC-Y2O3-Al2O3

Preparation of pressureless-sintered SiC-Y2O3-Al2O3
复制标题

无压烧结SiC-Y2O3-Al2O3的制备

DOI:
--
复制
发表时间:
1988
期刊:
影响因子:
--
通讯作者:
H. Takei
H. Takei
中科院分区:
--
文献类型:
--
作者:
M. Omori;H. Takei

文献摘要

被引文献

相似文献

以氢氧化铝和氢氧化钇为原料制备了烧结助剂。这些添加剂溶于水,形成粘结剂。将β-碳化硅粉末与添加剂溶液混合,在2150℃无压烧结。添加剂生成的氧化物促进了烧结。烧结体不含气孔。在烧结体中析出了铝、硅和氧化钇。
Sintering additives were prepared from aluminium hydroxide and yttrium hydroxide. These additives were soluble in water and resulted in a binder. A β-SiC powder was mixed with the additive solution and sintered at 2150° C without pressure. The oxides formed from the additive promoted sintering. The sintered body contained no pores. Aluminium, silicon, and yttrium oxide were precipitated in the sintered body.