Effect of microstructure on the mechanical properties of PAN-based carbon fibers during high-temperature graphitization
Effect of microstructure on the mechanical properties of PAN-based carbon fibers during high-temperature graphitization
复制标题
DOI:
10.1007/s10853-008-2633-y
复制
发表时间:
2008-06-01
影响因子:
4.5
通讯作者:
Zhu, Zhenping
中科院分区:
文献类型:
--
作者:
Liu, Fujie;Wang, Haojing;Zhu, Zhenping
The change of microstructure of PAN-based carbon fibers has been studied as a function of heat-treatment temperature (1,800-2,800 C, stretching 0%) by Raman spectroscopy and X-ray diffraction. With increasing heat-treatment temperature, both the crystallite size (L (a), L (c)) and the degree of preferred orientation (g) increase, while the crystallite interlayer spacing (d (002)) decreases. The values of both R (s) and R (c) decrease, while R (s) decreases more quickly. It implies that the degrees of skin-core of the carbon fibers increase. The relationship between mechanical properties and microstructure of the variants is also explored in detail.