Preparation of high purity uranium metal from aqueous solutions
Preparation of high purity uranium metal from aqueous solutions
复制标题
从水溶液中制备高纯金属铀
DOI:
10.1016/s0925-8388(96)02868-x
复制
发表时间:
1997
影响因子:
6.2
通讯作者:
K. Suzuki
中科院分区:
文献类型:
--
作者:
Y. Shiokawa;K. Hasegawa;K. Konashi;Masae Takahashi;K. Suzuki
The uranium amalgam was quantitatively prepared by electrolysis from the aqueous solution containing acetic acid and sodium acetate using a mercury cathode. A bright button or brown porous one of uranium metal was obtained by thermal decomposition of the amalgam. The purity was found to be much higher than commercial grade metal of ca. 99.95%. As a result of this work, the simple and easy procedure for preparation of uranium metal with a high level of purity on the laboratory scale has been developed.