Solution of Ni-Cr alloy oxides in an alkali alumino-silicate glass.
Solution of Ni-Cr alloy oxides in an alkali alumino-silicate glass.
复制标题
Ni-Cr 合金氧化物在碱金属铝硅酸盐玻璃中的溶液。
DOI:
10.1016/s0109-5641(88)80049-6
复制
发表时间:
1988
期刊:
影响因子:
--
通讯作者:
Baran,GR
中科院分区:
文献类型:
--
作者:
Baran,GR
During fusion of porcelain onto metal substrates, oxides on the alloy are dissolved by the glassy phase of the porcelain. The extent of solution needed for development of a bond has been discussed in theory, but measurements of oxide thickness and solubility have proven difficult to obtain. In this study, the interfacial compositions of Ni−Cr alloy/glass couples were determined using Auger analysis. The samples consisted of buttons of glass fused to 5 proprietary Ni−Cr alloys. After dissolution of the alloy by a 10% Br-methanol solution, the glass was analyzed. The diffusion profiles of elements in the oxide indicated incomplete dissolution of the oxide by the glass. High amounts of silicon were also found at the alloy/oxide interface.