Role of oxygen impurities in etching of silicon by atomic hydrogena)
Role of oxygen impurities in etching of silicon by atomic hydrogena)
复制标题
氧杂质在原子氢蚀刻硅中的作用)
DOI:
10.1116/1.2884731
复制
发表时间:
2008
期刊:
影响因子:
--
通讯作者:
M. Vepřek
中科院分区:
文献类型:
--
作者:
S. Vepřek;Chunlin Wang;M. Vepřek
In a pure-hydrogen glow discharge plasma, the etch rate of silicon increases with increasing temperature up to about ≥1100 A/s at 60–80 °C and, upon a further increase of the temperature, etch rate strongly decreases, showing Arrhenius-like dependence with negative apparent activation energy of −1.5 kcal/mol. When the Si sample is at the floating potential, oxygen impurities of ≥10 at. ppm strongly decrease the etch rate. At more than 70 ppm of oxygen, the etching stops. Oxygen adsorbed on the Si surface can be removed by ion bombardment when negative potential is applied to the Si sample and the Si is then etched chemically by H atoms. The etching by atomic hydrogen is isotropic in an oxygen-free system. A controllable addition of a few ppm of oxygen in combination with negative bias of the Si sample results in highly anisotropic etching with thin oxide acting as side-wall passivation.