Li, Xiang;Li, Xiansheng;Hao, Jiming
Ca poisoning and regeneration on V2O5-WO3/TiO2 catalysts for selective catalytic reduction of NOx was investigated based on the changes of activity, structure, reducibility, acidity and reaction details. It is found that high contents of CaO can lead to CaWO4 formation and thus passivate bulk tungsten species and surface acid sites of fresh catalyst. Additionally, reactable surface oxygen species and reducibility are also greatly suppressed by CaO species. However, unlike previous regeneration method, HEDP showed exclusive and excellent removal rate of CaO without large active ingredients loss, which had a better prospect of industrial application. (C) 2016 Published by Elsevier B.V.