Defects of large-size KDP single crystals and their influence on degradation of the optical properties
Defects of large-size KDP single crystals and their influence on degradation of the optical properties
复制标题
DOI:
10.1016/j.optmat.2006.11.003
复制
发表时间:
2007-09
影响因子:
3.9
通讯作者:
I. Pritula;M. Kolybayeva;V. I. Salo;V. Puzikov
中科院分区:
文献类型:
--
作者:
I. Pritula;M. Kolybayeva;V. I. Salo;V. Puzikov
It is shown that the developed method of solvent re-circulation, which provides optimum growth conditions at a constant temperature (Tcr=80°C, Vgrowth∼(0.8–1.6)×10−6cm/s, pH=4), allows to grow KDP crystals with a cross-section up to 300×300mm and a bulk laser damage threshold of ∼60J/cm2.