Hot deformation behavior and finite element simulation of Mg-8.3Gd-4.4Y-1.5Zn-0.8Mn alloy

Hot deformation behavior and finite element simulation of Mg-8.3Gd-4.4Y-1.5Zn-0.8Mn alloy
复制标题

Mg—8.3Gd—4.4Y—1.5Zn—0.8Mn合金的热变形行为及有限元模拟

DOI:
10.1016/j.jre.2021.05.005
复制
发表时间:
2022-04-27
影响因子:
4.9
通讯作者:
Yuan, Jiawei
Yuan, Jiawei
中科院分区:
化学2区
文献类型:
--
作者:
Fan, Jiabin;Ma, Minglong;Yuan, Jiawei

文献摘要

被引文献

相似文献

To study the hot deformation behavior of Mg-8.3Gd-4.4Y-1.5Zn-0.8Mn (wt%) alloy, hot compression tests were conducted using a Gleeble-350 0 thermal simulator at temperatures ranging from 653 to 773 K, true strain rates of 0.001-1 s(-1), and a deformation degree of 60%. Results of hot compression experiments show that the flow stress of the alloy increases with the strain rate. The true stress-true strain curves are corrected by correcting the effect of temperature rise in the deformation process. Activation energy, Q, equal to 287380 J/mol and material constant, n, equal to 4.59 were calculated by fitting the true stress-true strain curves. Then, the constitutive equation was established and verified via finite element simulation. Results of the hot processing map show that the probability of material instability increases with the degree of deformation, which indicates that the material is not suitable for large deformation in a single pass. On the whole, the alloy is appropriate for multipass processing with small deformation and a suitable processing temperature and strain rate are 733 K and 0.01 s(-1), respectively. (c) 2021 Chinese Society of Rare Earths. Published by Elsevier B.V. All rights reserved.