Nanocomposite-coated porous templates for engineered bone scaffolds: a parametric study of layer-by-layer assembly conditions

Nanocomposite-coated porous templates for engineered bone scaffolds: a parametric study of layer-by-layer assembly conditions
复制标题

DOI:
10.1088/1748-605x/ab3b7b
复制
发表时间:
2019-09
影响因子:
4
通讯作者:
M. Ziminska;Marine J Chalanqui;P. Chambers;J. Acheson;H. McCarthy;N. Dunne;A. Hamilton
M. Ziminska;Marine J Chalanqui;P. Chambers;J. Acheson;H. McCarthy;N. Dunne;A. Hamilton
中科院分区:
工程技术3区
文献类型:
--
作者:
M. Ziminska;Marine J Chalanqui;P. Chambers;J. Acheson;H. McCarthy;N. Dunne;A. Hamilton

文献摘要

相似文献

使用逐层(LbL)组装技术将机械增强涂层存款到多孔模板上是用于制造具有高孔隙率、强度和刚度的组合的工程化骨支架材料的途径。LbL组装涉及从水溶液中连续沉积纳米至微米尺度的多层涂层。在这里,使用实验设计(DOE)方法来评估聚乙烯亚胺(PEI)、聚丙烯酸(PAA)和纳米粘土涂层在开孔聚氨酯泡沫模板上的LbL组装。PAA溶液的pH值、盐浓度以及这些因素之间的相互作用对涂层的厚度、涂层泡沫模板的孔隙率、弹性模量和坍塌应力的影响最大。涂层泡沫的机械性能与涂层的厚度相关,但也归因于涂层性能的变化,由于不同的组装条件。DOE优化旨在平衡泡沫模板的较高机械性能和较低孔隙率之间的权衡,同时增加涂层厚度。微观力学建模预测,116个QL的沉积将在> 70%的合适孔隙率下实现松质骨的机械性能(>0.05 GPa刚度和>2 MPa强度)。当用PAA的最终层覆盖并通过热处理交联时,PEI/PAA/PEI/纳米粘土涂层表现出对间充质干细胞的良好的间接细胞毒性。LbL组装在多层结构涂层内存款广泛的功能成分的能力使得模板化LbL组装的一般策略成为用于制造工程化组织支架的有力途径,所述工程化组织支架可以施加到各种多孔模板材料上以实现广泛的性质、孔结构和多功能性。
Using the layer-by-layer (LbL) assembly technique to deposit mechanically reinforcing coatings onto porous templates is a route for fabricating engineered bone scaffold materials with a combination of high porosity, strength, and stiffness. LbL assembly involves the sequential deposition of nano- to micro-scale multilayer coatings from aqueous solutions. Here, a design of experiments (DOE) approach was used to evaluate LbL assembly of polyethyleneimine (PEI), polyacrylic acid (PAA), and nanoclay coatings onto open-cell polyurethane foam templates. The thickness of the coatings, and the porosity, elastic modulus and collapse stress of coated foam templates were most strongly affected by the pH of PAA solutions, salt concentration, and interactions between these factors. The mechanical properties of coated foams correlated with the thickness of the coatings, but were also ascribed to changes in the coating properties due to the different assembly conditions. A DOE optimization aimed to balance the trade-off between higher mechanical properties but lower porosity of foam templates with increasing coating thickness. Micromechanical modeling predicted that deposition of 116 QLs would achieve mechanical properties of cancellous bone (>0.05 GPa stiffness and >2 MPa strength) at a suitable porosity of >70%. When capped with a final layer of PAA and cross-linked via thermal treatment, the PEI/PAA/PEI/nanoclay coatings exhibited good indirect cytotoxicity with mesenchymal stem cells. The ability of LbL assembly to deposit a wide range of functional constituents within multilayer-structured coatings makes the general strategy of templated LbL assembly a powerful route for fabricating engineered tissue scaffolds that can be applied onto various porous template materials to achieve a wide range of properties, pore structures, and multifunctionality.