A new approach in interpreting the four-ball wear results
A new approach in interpreting the four-ball wear results
复制标题
解释四球磨损结果的新方法
DOI:
10.1016/0043-1648(62)90130-8
复制
发表时间:
1962
期刊:
影响因子:
5
通讯作者:
Feng I
中科院分区:
文献类型:
--
作者:
Feng I
An experimental study of the variation of wear volume as a function of test duration reveals that the four-ball wear process very frequently follows through three characteristic stages: (1) the “running-in” period, (2) the steady-state wear, and (3) the equilibrium stage. The amount of “running-in” wear, the steady-state wear rate and the equilibrium scar size can be determined from the log—log plot of the scar diameter against the test duration. Thus, the logdvs.logtcurve provides a convenient way of comparing the wear performances of various lubricants.